Clin Wax
Powdered wax for flat work ironers
Take a bed sheet, which is as wide as the cylinder. Put 150 – 200 g Clin Wax and fold it up. Put same quantities on each corner.
Heat the ironer up to 150 - 200°C and pass the sheet 3 – 4 times through the cylinder.
Afterwards pass 3 – 4 sheets, which are out of use, through the cylinder and continue with normal ironing process.
This application should be done every morning or every 8 hours depending on working time of the ironer.
Product Detail
Packaging Net 3 kg bucket